Grinding of . Granulated Copper Slag Before grinding, the granulated copper slag was dried using the oven at a temperature of 100 o C for 24 hours. Afterwards, this copper slag was intensively ground using a ball mill. To obtain two level of fineness, a short duration (5 minutes) and long duration (1 .